WebMar 21, 2024 · The processes that limit repeated rejuvenation of directionally solidified GTD444 and single-crystal René N5 (SX) alloys have been studied in detail. A rejuvenation cycle includes a rejuvenation heat treatment and/or small-scale material removal, followed by creep or fatigue testing. WebJan 10, 2024 · Wu et al. [ 19] found the formation of lamellar borides at grain boundaries in the directionally solidified superalloys with 0.03 wt. % boron, which would make the interfaces brittle and decrease the rupture life of material.
Directional solidification of Ni-based superalloy castings: …
WebThe present conference discusses topics in P/M and wrought superalloys, alternatives to superalloys, directionally-solidified and single-crystal alloys, advancements in … WebInfluence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2024, 56(7): 969-978. ... Effect of Longitudinal Static Magnetic Field on the Columnar to Equiaxed Transition in Directionally Solidified GCr15 Bearing Steel[J]. 金属学报, 2024, 54(5): 801-808. [15] can westfield gift cards be used anywhere
Thermomechanical Fatigue Behavior of a Directionally Solidified …
WebJan 11, 2024 · Nickel-base superalloys exhibit high strength, good resistance to corrosion and oxidation, long fatigue life and is capable of withstanding high temperatures for extended periods of time. Consequently, Ni-base superalloys (NBSAs) are highly suitable as blading materials. WebJan 1, 2024 · Directional solidified (DS) superalloys Creep resistance of superalloys is increased if manufactured by the DS method. This is because of grain boundaries being formed vertically and hence they are less susceptible to the centrifugal force of the turbine blades. Polycrystalline alloy Mar-M200 is directionally solidified to form Mar-M200 Hf … WebKeywords: Directional solidification, Hot tearing, Ni-based superalloys Abstract The hot tearing mechanism has been studied in directionally solidified (DS) Ni-based superalloys with columnar grain structures. Castability tests and optical metallography of quenched samples were employed to explore the effect of microstructural can westfield vouchers be used anywhere